Material Notes:
TPE-SInformation provided by BARLOG plastics GmbH.
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.028 cm/cm
0.028 in/in
ISO 294-4
Linear Mold Shrinkage, Transverse 0.0040 cm/cm
0.0040 in/in
ISO 294-4
Mechanical Properties Metric English Comments
Hardness, Shore A 45
45
Tensile Strength at Break 3.60 MPa
522 psi
ISO 527-1
Elongation at Break 620 %
620 %
ISO 527-1
Descriptive Properties Value Comments
Resin Type TPE-S
Users viewing this material also viewed the following: