Barlog Plastics KEBAFLEX S 25 A.01 TPE-S, Shore A25, translucent

Category Polymer , Thermoplastic , Elastomer, TPE , Styrenic TPE
Manufacturer Barlog Plastics
Trade Name KEBAFLEX
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Barlog Plastics KEBAFLEX S 25 A.01 TPE-S, Shore A25, translucent.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TPE-SInformation provided by BARLOG plastics GmbH.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.047 cm/cm
0.047 in/in
ISO 294-4
Linear Mold Shrinkage, Transverse 0.013 cm/cm
0.013 in/in
ISO 294-4
Mechanical Properties Metric English Comments
Hardness, Shore A 25
25
Tensile Strength at Break 2.10 MPa
305 psi
ISO 527-1
Elongation at Break 370 %
370 %
ISO 527-1
Descriptive Properties Value Comments
Resin Type TPE-S