Bapolene® PP5062 Polypropylene, Injection Grade

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Bapolene®
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Bapolene® PP5062 Polypropylene, Injection Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polypropylene injection impact copolymer with excellent color and processability. This resin offers a superior balance of stiffness and impact strength. This product meets the FDA requirements of 21CFR 177.1520.Applications: Housewares, appliances, battery cases, office furniture, toys, consumer products.Bapolene® and Bapolan® are registered trademarks of Bamberger Polymers, Inc. Information provided by Bamberger Polymers.
Physical Properties Metric English Comments
Density 0.905 g/cc
0.0327 lb/in³
ASTM D1505
Melt Flow 12 g/10 min

@Load 2.16 kg,
Temperature 230 °C
12 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 83
83
ASTM D2240
Tensile Strength, Yield 27.6 MPa
4000 psi
50 mm/min (2 in./min.); ASTM D638
Elongation at Break >= 200 %
>= 200 %
50 mm/min (2 in./min.); ASTM D638
Elongation at Yield 14 %
14 %
50 mm/min (2 in./min.); ASTM D638
Flexural Modulus 1.24 GPa
180 ksi
Secant @ 1% strain; ASTM D790
Izod Impact, Notched 1.33 J/cm
2.50 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 103 °C
217 °F
ASTM D648
Descriptive Properties Value Comments
Process Injection Molding
Region Europe/Turkey
Bamberger Polymers Distribution