Bapolene PP4071 is a high flow PP homopolymer for staple and continuous filament applications as well as general purpose injection molding. This resin exhibits good melt and thermal stability.Applications: Upholstery, BCF carpet yarns, multifilament, general purpose injection molding.Bapolene® and Bapolan® are registered trademarks of Bamberger Polymers, Inc. Information provided by Bamberger Polymers
Physical Properties Metric English Comments
Density 0.901 g/cc
0.0326 lb/in³
ASTM D1505
Melt Flow 18 g/10 min

@Load 2.16 kg,
Temperature 230 °C
18 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 18.6 MPa
2700 psi
2 in/min (50 mm/min); ASTM D638
Tensile Strength, Yield 35.2 MPa
5110 psi
2 in/min (50 mm/min); ASTM D638
Elongation at Break 20 %
20 %
2 in/min (50 mm/min); ASTM D638
Elongation at Yield 9.0 %
9.0 %
2 in/min (20 mm/min); ASTM D638
Flexural Modulus 1.45 GPa
210 ksi
Secant @ 1% strain; ASTM D-790
Izod Impact, Notched 0.240 J/cm
0.450 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 99.0 °C
210 °F
ASTM D648
Descriptive Properties Value Comments
Process Fiber
Injection Molding
Region Europe/Turkey
International