Bapolene® 2292 Polyethylene Film Grade

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE
Manufacturer Bapolene®
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Bapolene® 2292 Polyethylene Film Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Bapolene 2292 is a butene linear low density polyethylene copolymer designed to provide a combination of toughness and stiffness and complies with FDA 21 CFR177.1520.Applications: Closures, lids, and housewares.All data is based on molded plaques.Bapolene® and Bapolan® are registered trademarks of Bamberger Polymers, Inc. Information provided by Bamberger Polymers
Physical Properties Metric English Comments
Density 0.925 g/cc
0.0334 lb/in³
ASTM D-1505
Melt Flow 50 g/10 min
50 g/10 min
ASTM D-1228
Mechanical Properties Metric English Comments
Hardness, Shore D 50
50
ASTM D-2240
Tensile Strength, Yield 10.7 MPa
1550 psi
ASTM D-638
Elongation at Break 90 %
90 %
ASTM D-638
Flexural Modulus 0.387 GPa
56.1 ksi
ASTM D-790
Descriptive Properties Value Comments
Process Injection Molding
Region Europe/Turkey
Bamberger Polymers Distribution
International
Bamberger Polymers Distribution
Mexico
Bamberger Polymers Distribution
US & Canada
Bamberger Polymers Distribution
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved