Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Bapolene® 108A Low Density Polyethylene Film Extrusion Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE
Manufacturer Bapolene®
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Bapolene® 108A Low Density Polyethylene Film Extrusion Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Bapolene® 108A is an LDPE for blown film. It contains 2500 ppm antiblock additive. This product meets the Food and Drug Administration requirements of 21CFR177.1520.Applications: General purpose packaging.Information provided by Bamberger Polymers.
Physical Properties Metric English Comments
Density 0.925 g/cc
0.0334 lb/in³
ASTM D-1505
Thickness 31.8 microns
1.25 mil
as tested; 2.5:1 BUR
Melt Flow 0.80 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.80 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D-1238
Antiblock Level 2500 ppm
2500 ppm
target
Mechanical Properties Metric English Comments
Dart Drop 3.78 g/micron
96.0 g/mil
F<sub>50</sub>; ASTM D-1709
Dart Drop Test 120 g

@Thickness 0.0317 mm
0.265 lb

@Thickness 0.00125 in
F<sub>50</sub>; ASTM D-1709
1% Secant Modulus, MD 179 MPa

@Thickness 0.0317 mm
26000 psi

@Thickness 0.00125 in
ASTM D-882
1% Secant Modulus, TD 221 MPa

@Thickness 0.0317 mm
32000 psi

@Thickness 0.00125 in
ASTM D-882
Optical Properties Metric English Comments
Haze 7.0 %

@Thickness 0.0317 mm
7.0 %

@Thickness 0.00125 in
ASTM D-1003
Descriptive Properties Value Comments
Process Film
Region Europe/Turkey
Bamberger Polymers Distribution
International
Bamberger Polymers Distribution
Mexico
Bamberger Polymers Distribution
US & Canada
Bamberger Polymers Distribution
Users viewing this material also viewed the following: