Material Notes:
This resin is a high density polyethylene homopolymer for blow molding applications. It is recommended for applications that require high top load strength and good stiffness. This product meets 21CFR177.1520.Applications: Blow molded containers, milk, juice, and water bottles.Bapolene® and Bapolan® are registered trademarks of Bamberger Polymers, Inc. Information provided by Bamberger Polymers
Physical Properties Metric English Comments
Density 0.960 g/cc
0.0347 lb/in³
ASTM D1505
ESCR 100% Igepal® 10 hour
10 hour
Melt Flow 0.70 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.70 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 31.0 MPa
4500 psi
2 in/min (50 mm/min); ASTM D638
Elongation at Break >= 300 %
>= 300 %
2 in/min (50 mm/min); ASTM D638
Flexural Modulus 1.55 GPa
225 ksi
Tangent Method 1; ASTM D-790
Descriptive Properties Value Comments
Process Blow Molding
Region Europe/Turkey
Bamberger Polymers Distribution
International
Bamberger Polymers Distribution
Mexico
Bamberger Polymers Distribution
US & Canada
Bamberger Polymers Distribution
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved