Bales Mold Service Nicklon® Nickel-P.T.F.E. Mold Coating

Category Metal , Metal Matrix Composite , Nonferrous Metal , Nickel Alloy , Other Engineering Material , Ceramic/Metallic Coating
Manufacturer Bales Mold Service
Trade Name Nicklon®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Bales Mold Service Nicklon® Nickel-P.T.F.E. Mold Coating.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Autocatalytic application provides a uniform layer of 22%-24% PTFE over the deepest ribs and most complex details. It is also corrosion resistant.Excellent Release Properties for: Deep Ribs"No Draft" CoresTextured SurfacesDifficult to Eject PolymersInformation provided by Bales Mold Service Inc.
Mechanical Properties Metric English Comments
Hardness, Rockwell C 45
45
Coefficient of Friction <= 0.10
<= 0.10
Processing Properties Metric English Comments
Processing Temperature 85.0 °C
185 °F
Applied Temperature