Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

BYK Cloisite® 93A Nanoclay

Category Other Engineering Material , Additive/Filler for Polymer , Polymer
Manufacturer BYK Additives
Trade Name Cloisite®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BYK Cloisite® 93A Nanoclay.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Cloisite® 93A is an additive for plastics to improve various plastic physical properties, such as reinforcement, HDT, CLTE and barrier.Information provided by Southern Clay ProductsSouthern Clay Products is now a part of BYK Additives.
Physical Properties Metric English Comments
Specific Gravity 1.88 g/cc
1.88 g/cc
Bulk Density 0.1692 g/cc
0.006111 lb/in³
Loose
0.2888 g/cc
0.01043 lb/in³
Packed
Loss On Ignition 40 %
40 %
Particle Size <= 2.0 µm
<= 2.0 µm
10%
<= 6.0 µm
<= 6.0 µm
50%
<= 13 µm
<= 13 µm
90%
Mechanical Properties Metric English Comments
Hardness, Shore D 83
83
5% Cloisite® reinforced Nylon 6
Tensile Strength, Ultimate 101 MPa
14600 psi
5% Cloisite® reinforced Nylon 6
Elongation at Break 8.0 %
8.0 %
5% Cloisite® reinforced Nylon 6
Modulus of Elasticity 4.657 GPa
675.5 ksi
5% Cloisite® reinforced Nylon 6
Flexural Modulus 3.78 GPa
548 ksi
5% Cloisite® reinforced Nylon 6
Izod Impact, Notched 0.270 J/cm
0.506 ft-lb/in
5% Cloisite® reinforced Nylon 6
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 96.0 °C
205 °F
5% Cloisite® reinforced Nylon 6
Processing Properties Metric English Comments
Moisture Content <= 2.0 %
<= 2.0 %
Descriptive Properties Value Comments
Modifier Concentration, meq/ 100g clay 90
Organic Modifier methyl, dihydrogenated tallow ammonium
X-Ray Diffraction d-Spacing (001) 23.6 Angstroms
Copyright © lookpolymers.com All Rights Reserved