Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

BNZ Materials Super Blakbond Mortar

Category Ceramic , Oxide , Silicon Oxide
Manufacturer BNZ Materials, Inc.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BNZ Materials Super Blakbond Mortar.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Super Blakbond is an air-setting mortar for general purpose plant use. It has greater air-setting strength than Blakbond or No. 2986. It is good for insulating fire brick where greater bond strength is desired, and can also be used for dense fire brick. Super Blakbond is particularly good for deep patching. It is also used for coating over industrial boiler tubes to level the surface and for shallow patching. The overall excellent properties of Super Blakbond make it ideal for the one mortar to carry in plant inventory. Temperature to 3000°F. An excellent choice for the one mortar on a job involving dense fire brick and insulating fire brick.Information provided by BNZ Materials Inc.
Physical Properties Metric English Comments
Bulk Density 1.99 g/cc
0.0718 lb/in³
Dipping, 4% H2O
2.02 g/cc
0.0729 lb/in³
As received
Mechanical Properties Metric English Comments
Modulus of Rupture 0.00259 GPa
0.376 ksi
Dipped Joint; ASTM C198
0.0290 GPa
4.21 ksi
Mortar
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 1650 °C
3000 °F
Shrinkage 4.3 %
4.3 %
Permanent Linear Change at Use Limit
Component Elements Properties Metric English Comments
Al2O3 43.2 %
43.2 %
CaO 0.30 %
0.30 %
Fe2O3 1.2 %
1.2 %
K2O 0.80 %
0.80 %
Loss on Ignition(%) 1.8 %
1.8 %
Na2O 2.4 %
2.4 %
SiO2 48.8 %
48.8 %
TiO2 1.5 %
1.5 %
Users viewing this material also viewed the following: