Material Notes:
375-L Insulating Cement used specifically in the aluminum industry as a filler material and trough liner, 375-L Insulating Cement is a 1500°F product Typical Applications: Insulating and Sealing: For kiln and furnace refractory crowns and domes, and flat suspended arches. Insulation of small steel pipe fittings
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 816 °C
1500 °F
Descriptive Properties Value Comments
Color White