BLUESTAR 203G30 PBT, 30% Glass Filled

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled
Manufacturer BLUESTAR
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BLUESTAR 203G30 PBT, 30% Glass Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Typical Applications: Thinner wall partsInformation provided by Polymer Technology and Services, LLC (PTS).
Physical Properties Metric English Comments
Specific Gravity 1.61 g/cc
1.61 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0040 cm/cm
0.0040 in/in
ASTM D955
Linear Mold Shrinkage, Transverse 0.0080 cm/cm
0.0080 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 105 MPa
15200 psi
ASTM D638
Flexural Strength 163 MPa
23600 psi
ASTM D790
Flexural Modulus 8.90 GPa
1290 ksi
ASTM D790
Izod Impact, Notched (ISO) 11.0 kJ/m²
5.23 ft-lb/in²
ASTM D256
Izod Impact, Unnotched (ISO) 45.0 kJ/m²
21.4 ft-lb/in²
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 203 °C
397 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 0.800 mm
V-0

@Thickness 0.0315 in
V-0

@Thickness 1.60 mm
V-0

@Thickness 0.0630 in
V-0

@Thickness 3.20 mm
V-0

@Thickness 0.126 in
Users viewing this material also viewed the following: