BCC Products DP-11-75 Urethane Adhesive

Category Polymer , Adhesive , Thermoset , Polyurethane, TS , Thermoset Polyurethane, Adhesive
Manufacturer BCC Products
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BCC Products DP-11-75 Urethane Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DP-11-75 is a two component medium viscosity urethane patch system. A hybrid product which was designed specifically for making quick responsive repairs/buildups to the MB 4000 Foundry Plank. DP-11-75 is exceptionally tough, highly machinable after cure, and exhibits superior properties similar to MB 4000.Information provided by BCC Products, Inc.
Physical Properties Metric English Comments
Brookfield Viscosity 200 cP
200 cP
Part A
1600 cP
1600 cP
Part B
Processing Properties Metric English Comments
Cure Time 20.0 - 30.0 min
0.333 - 0.500 hour
Pot Life 1.5 min

@Temperature 24.0 °C
1.5 min

@Temperature 75.2 °F
20 gram mass
Descriptive Properties Value Comments
Mix Ratio 1:1 by volume