Material Notes:
BC7136-2 is an aluminum filled thick section casting system with heat resistance to 300ºF. May be cast to a thickness of 2 inches in non-conductive molds, 3 inches in conductive molds and thicker sections with the addition of bulk fill. For service temperature above 150ºF a post-cure is required. Does not contain VCHD or MDA. See cure schedule.Information provided by BCC Products, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.67 g/cc
1.67 g/cc
Brookfield Viscosity 13500 cP

@Temperature 23.9 °C
13500 cP

@Temperature 75.0 °F
Mixed
Linear Mold Shrinkage 0.0010 cm/cm
0.0010 in/in
ASTM D2566-69
Mechanical Properties Metric English Comments
Hardness, Shore D 90

@Temperature 23.9 °C
90

@Temperature 75.0 °F
Tensile Strength, Ultimate 54.5 MPa
7900 psi
Flexural Strength 61.4 MPa
8900 psi
Compressive Strength 190 MPa
27600 psi
Thermal Properties Metric English Comments
CTE, linear 36.4 µm/m-°C
20.2 µin/in-°F
Deflection Temperature at 1.8 MPa (264 psi) 157 °C
314 °F
Processing Properties Metric English Comments
Cure Time 1440 min

@Temperature 24.0 °C
24.0 hour

@Temperature 75.2 °F
Pot Life 180 min

@Temperature 24.0 °C
180 min

@Temperature 75.2 °F
1 lb. mass
Descriptive Properties Value Comments
Mix Ratio 100:9 by weight, 100:16 by volume, resin/harder