Material Notes:
BC 7062 are aluminum filled, low viscosity epoxy mass casting resins. These room temperature cure systems allow the user choice thicknesses of 1/8 inch to a maximum of 6 inches without foaming or yielding excessive shrinkage. Casting thicknesses may be increased by incorporating aluminum needles, puffs or granules. BC 7062, when properly cured, provides nearly perfect reproduction, resulting in a dimensionally stable, hard, tough surface. For use in constructing duplicate models, prototypes, patterns, facing dies, etc.Information provided by BCC Products, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.85 g/cc
1.85 g/cc
Brookfield Viscosity 5400 cP

@Temperature 23.9 °C
5400 cP

@Temperature 75.0 °F
Mixed
Linear Mold Shrinkage 0.0012 cm/cm
0.0012 in/in
ASTM D2566-69
Mechanical Properties Metric English Comments
Hardness, Shore D 86

@Temperature 23.9 °C
86

@Temperature 75.0 °F
Tensile Strength, Ultimate 36.5 MPa
5300 psi
Flexural Strength 60.7 MPa
8800 psi
Compressive Strength 99.3 MPa
14400 psi
Thermal Properties Metric English Comments
CTE, linear 57.6 µm/m-°C
32.0 µin/in-°F
Heat Distortion Temperature 56.7 °C
134 °F
Processing Properties Metric English Comments
Cure Time 720 - 1080 min

@Temperature 24.0 °C
12.0 - 18.0 hour

@Temperature 75.2 °F
Pot Life 50 - 60 min

@Temperature 24.0 °C
50 - 60 min

@Temperature 75.2 °F
2 lb. mass
Descriptive Properties Value Comments
Machinability Excellent
Mix Ratio 12:1 by weight, 6.5:1 by volume, resin/harder