Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

BCC Products BC 6005 Epoxy Surface Coat

Category Polymer , Thermoset , Epoxy
Manufacturer BCC Products
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BCC Products BC 6005 Epoxy Surface Coat.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
BC 6005 is a snow white thixotropic epoxy resin designed specifically for quality reproduction of a variety of surfaces. A room temperature cure system that offers ample working time yet affords quick-tack for lamination. BC 6005 may be applied easily with a brush or troweled to a thickness of 1/8” or less on vertical surfaces or over sharp radii without sag or fear of run-off. When cured, this resin system provides a hard tough chip-resistant surface.Information provided by BCC Products, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.50 g/cc
1.50 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore D 89

@Temperature 25.0 °C
89

@Temperature 77.0 °F
Tensile Strength, Ultimate 46.9 MPa
6800 psi
Flexural Strength 61.4 MPa
8900 psi
Flexural Modulus 6.62 GPa
960 ksi
Compressive Strength 90.3 MPa
13100 psi
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 58.9 °C
138 °F
Processing Properties Metric English Comments
Cure Time 480 - 720 min

@Temperature 24.0 °C
8.00 - 12.0 hour

@Temperature 75.2 °F
Pot Life 18 - 22 min

@Temperature 24.0 °C
18 - 22 min

@Temperature 75.2 °F
4 oz. mass
Descriptive Properties Value Comments
Mix Ratio 6:1 by weight, 4:1 by volume, resin/harder
Mixed Viscosity, Brookfield Thixotropic
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved