Material Notes:
BC4553 is designed for instant buildup and repair of plastic surfaces and models. Recommended for use on SMC and FRP parts, vacuum form molds and a variety of surfaces. When cured BC4553 produces a hard, strong, chip resistant, tack-free surface. Area to be filled should be clean and dry, free from dust, oil and release agents. It is advisable to scarify the area prior to application. May be applied at any reasonable thickness by spreading or splining. Do not work with more material than can be applied in 5 minutes. Material mixed with cream hardener should not be returned to original can. After final cure material may be scraped, sanded, filed, drilled, taped or machined to a featheredge. Available in Ultra-white, gray, pine and mahoganyInformation provided by BCC Products, Inc.
Processing Properties Metric English Comments
Cure Time 20.0 - 60.0 min

@Temperature 24.0 °C
0.333 - 1.00 hour

@Temperature 75.2 °F
Pot Life 5.0 - 10 min

@Temperature 24.0 °C
5.0 - 10 min

@Temperature 75.2 °F
1lb mass
Shelf Life 6.00 Month
6.00 Month
in tightly closed container
Descriptive Properties Value Comments
Mix Ratio 100:1 or 100:2 resin/hardener
Mixed Viscosity, Brookfield Thixotropic