Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

BASF Ultramid® SEGM35 H1 BK 6259 40% Glass/Mineral Filled PA6 (Dry)

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Glass/Mineral Reinforced
Manufacturer BASF
Trade Name Ultramid®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Ultramid® SEGM35 H1 BK 6259 40% Glass/Mineral Filled PA6 (Dry).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Ultramid SEGM35 H1 BK6259 is a 40% glass/mineral reinforced injection molding grade. It offers enhanced surface appearance, it also exhibits similar UV weathering characteristics compared to 8267G HS BK-106. In parts containing cross sections, significant pressure drops are encountered during filling.Applications: Mirror housings, rear liftgate handles and luggage rack components.Information provided by BASF
Physical Properties Metric English Comments
Density 1.48 g/cc
0.0535 lb/in³
ISO 1183
Moisture Absorption at Equilibrium 0.90 %
0.90 %
24 Hours; ISO 62
1.6 %
1.6 %
50% RH; ISO 62
5.7 %
5.7 %
Saturation; ISO 62
Melt Flow 39.42 g/10 min
39.42 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 80.0 MPa
11600 psi
ISO 527
Flexural Modulus 4.80 GPa
696 ksi
ISO 178
Izod Impact, Notched (ISO) 2.40 kJ/m²
1.14 ft-lb/in²
ISO 180
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 144 °C
291 °F
ISO 75
Processing Properties Metric English Comments
Melt Temperature 270 - 295 °C
518 - 563 °F
Mold Temperature 80.0 - 95.0 °C
176 - 203 °F
Dry Time 2 - 4 hour
2 - 4 hour
Moisture Content <= 0.10 %
<= 0.10 %
Descriptive Properties Value Comments
Color BK 6259
Commercial Status North America
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved