BASF Ultramid® B27 E PA6

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Unreinforced
Manufacturer BASF
Trade Name Ultramid®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Ultramid® B27 E PA6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Ultramid® B27 E is a polyamide 6 grade of low viscosity that is well suited for compounding and the production of monofilaments. Product comes in 2-2.5 mm round pellets.Information provided by BASF