BASF Ultramid® A3K BK 00464 PA66 (Conditioned)

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Unreinforced
Manufacturer BASF
Trade Name Ultramid®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Ultramid® A3K BK 00464 PA66 (Conditioned).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Easy flowing injection-molding grade for fast processing. Uses include highly stressed technical parts such as bearings and gear wheels; also electrically insulating parts such as terminals and cable connectors, as Fc grade suitable for food contact.Information provided by BASF
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
ISO 1183
Water Absorption 8.0 - 9.0 %
8.0 - 9.0 %
Saturation; ISO 62
Moisture Absorption at Equilibrium 2.5 - 3.1 %
2.5 - 3.1 %
23°C; 50% RH; ISO 62
Viscosity Measurement 150
150
ISO 307
Linear Mold Shrinkage 0.0085 cm/cm
0.0085 in/in
restricted
Melt Flow 129.95 g/10 min

@Load 5.00 kg,
Temperature 275 °C
129.95 g/10 min

@Load 11.0 lb,
Temperature 527 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 50.0 MPa
7250 psi
50 mm/min; ISO 527-1/-2
Elongation at Yield 20 %
20 %
50 mm/min; ISO 527-1/-2
Modulus of Elasticity 1.10 GPa
160 ksi
ISO 527-1/-2
Izod Impact, Notched (ISO) NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ISO 180/A
Charpy Impact Unnotched NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 2.00 J/cm²

@Temperature 23.0 °C
9.52 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Tensile Creep Modulus, 1000 hours 700 MPa
102000 psi
ISO 899-1
Thermal Properties Metric English Comments
Specific Heat Capacity 1.70 J/g-°C
0.406 BTU/lb-°F
Thermal Conductivity 0.330 W/m-K
2.29 BTU-in/hr-ft²-°F
DIN 52612
Melting Point 260 °C
500 °F
DIN 53765
Maximum Service Temperature, Air 101 °C
214 °F
for 50% loss of tensile strength after 20000hr
118 °C
244 °F
for 50% loss of tensile strength after 5000hr
200 °C
392 °F
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+10 ohm-cm
1.00e+10 ohm-cm
IEC 60093
Surface Resistance 1.00e+10 ohm
1.00e+10 ohm
IEC 60093
Dielectric Constant 5.0

@Frequency 1.00 Hz
5.0

@Frequency 1.00 Hz
IEC 60250
Dissipation Factor 0.00020

@Frequency 1.00e+6 Hz
0.00020

@Frequency 1.00e+6 Hz
IEC 60250
Comparative Tracking Index 600 V
600 V
Test solution A; IEC 60112
Processing Properties Metric English Comments
Melt Temperature 280 - 300 °C
536 - 572 °F
Injection-molding/Extrusion
Mold Temperature 60.0 - 80.0 °C
140 - 176 °F
Injection-molding
Descriptive Properties Value Comments
Color BK 00464
Commercial Status Europe
Copyright © lookpolymers.com All Rights Reserved