Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

BASF Ultramid® A3EG7 BK23189 35% Glass Filled PA66 (Dry)

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 40% Glass Fiber Filled
Manufacturer BASF
Trade Name Ultramid®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Ultramid® A3EG7 BK23189 35% Glass Filled PA66 (Dry).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Ultramid A3EG6 BK23189 is a 35% glass fiber reinforced injection molding PA66 grade for machinery components and housings of high stiffness and dimensional stability.
Physical Properties Metric English Comments
Density 1.41 g/cc
0.0509 lb/in³
ISO 1183
Water Absorption 1.6 %
1.6 %
24 hour; ISO Test
5.0 %
5.0 %
ISO 62
Moisture Absorption at Equilibrium 1.6 %
1.6 %
23°C/50% R.H.; ISO 62
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 190 MPa
27600 psi
5mm/min; ISO 527
Elongation at Break 2.8 %
2.8 %
5mm/min; ISO 527
Izod Impact, Notched (ISO) 9.50 kJ/m²
4.52 ft-lb/in²
ISO Test
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
10 K/min
260 °C
500 °F
ASTM Test
Deflection Temperature at 1.8 MPa (264 psi) 250 °C
482 °F
ISO 75
Descriptive Properties Value Comments
Color BK23189
Commercial Status Active America
Impact Modified No
Primary Processing Technique Injection Molding
Users viewing this material also viewed the following: