Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

BASF Ultramid® 8267G HS BK-106A 15/25% Glass/Mineral Filled PA6 (Conditioned)

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Glass/Mineral Reinforced
Manufacturer BASF
Trade Name Ultramid®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Ultramid® 8267G HS BK-106A 15/25% Glass/Mineral Filled PA6 (Conditioned).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Ultramid 8267G HS BK-106A is a heat stabilized, weather resistant, 40% mineral and glass fiber reinforced PA6 injection molding compound with improved UV resistance and sink mark resistance. The combination of mineral and glass fibers result in a high performance, low warp and cost effective engineering thermoplastic. It exhibits high strength, good UV resistance, rigidity and good heat distortion temperatures. It has a relatively high resistance to creep under load. The heat stabilizer system extends its retention of properties at elevated temperatures. It has good chemical resistance to greases, oils and hydrocarbons.
Physical Properties Metric English Comments
Density 1.48 g/cc
0.0535 lb/in³
dry; ISO 1183
Water Absorption 0.90 %
0.90 %
24 hour; ISO Test
5.7 %
5.7 %
beginning dry; ISO 62
Moisture Absorption at Equilibrium 1.6 %
1.6 %
beginning dry (23°C/50% R.H.); ISO 62
Linear Mold Shrinkage 0.0040 cm/cm
0.0040 in/in
ASTM Data; MD
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
10 K/min
220 °C
428 °F
ASTM Test
Descriptive Properties Value Comments
Color BK-106A
Commercial Status Active America
Impact Modified No
Primary Processing Technique Injection Molding
UL.UL-C Yes