Material Notes:
Description Ultramid 8234G HS BK-102 is heat stabilized, pigmented black, 44% glass reinforced PA6 injection molding compound offering the highest level of strength, stiffness, high temperature performance and dimensional stability. Its resistance to creep under load is excellent. It maintains its inherent chemical resistance to greases, oils and hydrocarbons. It is available in natural and black versions. Pigmented and weatherable versions may be offered on a case by case basis.Applications: consumer power tool housings, cattle ear taggers, luggage frames, fans and pressure regulator housings.Information provided by BASF
Physical Properties Metric English Comments
Density 1.49 g/cc
0.0538 lb/in³
ISO 1183
Moisture Absorption at Equilibrium 0.90 %
0.90 %
24 hour; ISO 62
1.5 %
1.5 %
50% RH; ISO 62
5.2 %
5.2 %
Saturation; ISO 62
Processing Properties Metric English Comments
Melt Temperature 280 - 305 °C
536 - 581 °F
Mold Temperature 80.0 - 95.0 °C
176 - 203 °F
Dry Time 2 - 4 hour
2 - 4 hour
Moisture Content <= 0.060 %
<= 0.060 %
Descriptive Properties Value Comments
Color BK 102
Commercial Status North America