Material Notes:
Description: Ultramid® 1C forms flexible, scratch-resistant coatings or tough, resilient, abrasion-resistant coverings on plastics, films, nonwovens, fabrics, leather, paper, wood, or metal.Information provided by BASF
Physical Properties Metric English Comments
Bulk Density 0.500 - 0.800 g/cc
0.0181 - 0.0289 lb/in³
Density 1.10 g/cc
0.0397 lb/in³
Mechanical Properties Metric English Comments
Ball Indentation Hardness 115 MPa
16700 psi
ISO 2039/1
Tensile Modulus 2.40 GPa
348 ksi
ISO 527
Flexural Strength 100 MPa
14500 psi
ISO 178
Flexural Modulus 2.30 GPa
334 ksi
ISO 178
Charpy Impact Unnotched 15.0 J/cm²
71.4 ft-lb/in²
ISO 179/1eU
Thermal Properties Metric English Comments
Melting Point 185 °C
365 °F
Glass Transition Temp, Tg 73.0 °C
163 °F
Decomposition Temperature >= 300 °C
>= 572 °F
Descriptive Properties Value Comments
Commercial Status Europe
Ignition Temperature >400°C
ASTM D1929