Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

BASF Ultradur B 4300 G2 LS High Speed BK15045 10% Glass Filled PBT

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled
Manufacturer BASF
Trade Name Ultradur B
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Ultradur B 4300 G2 LS High Speed BK15045 10% Glass Filled PBT.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Density 1.38 g/cc
0.0499 lb/in³
ISO 1183
Viscosity Test 104 cm³/g
104 cm³/g
Viscosity number
Melt Flow 35 g/10 min

@Load 2.16 kg,
Temperature 250 °C
35 g/10 min

@Load 4.76 lb,
Temperature 482 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 85.0 MPa
12300 psi
5mm/min; ISO 527
Elongation at Break 3.6 %
3.6 %
5mm/min; ISO 527
Tensile Modulus 4.56 GPa
661 ksi
1mm/min; ISO 527
Thermal Properties Metric English Comments
Melting Point 223 °C
433 °F
10 K/min
Deflection Temperature at 0.46 MPa (66 psi) 215 °C
419 °F
ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 184 °C
363 °F
ISO 75
Descriptive Properties Value Comments
Color BK15045
Commercial Status Active America
Impact Modified No
Primary Processing Technique Injection Molding
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved