Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

BASF Ultradur B 4040 G3 HT BK5830 15% Glass Filled PBT/PET

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , PBT + PET Blend, Glass Filled , Polyethylene Terephthalate (PET)
Manufacturer BASF
Trade Name Ultradur B
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Ultradur B 4040 G3 HT BK5830 15% Glass Filled PBT/PET.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Ultradur B 4040 G3 HT BK5830 is a 15% glass filled, pigmented black, injection molding PBT. It is a resin for molding household appliances and equipment which must be resistant to chemicals and other media, and be capable of producing a excellent surface finish. In addition, some types of kitchen equipment have to with-stand high temperatures. B4040G3 HT's resistance to high sustained-service temperatures makes it a material of choice when things get hot. Internal testing demonstrates that the product meets the UL94 HB (0.8 mm thickness) flame requirements.
Physical Properties Metric English Comments
Density 1.42 g/cc
0.0513 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0050 cm/cm
0.0050 in/in
ISO Data
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 70.0 MPa
10200 psi
5mm/min; ISO 527
Elongation at Break 1.5 %
1.5 %
5mm/min; ISO 527
Tensile Modulus 6.00 GPa
870 ksi
1mm/min; ISO 527
Flexural Modulus 5.50 GPa
798 ksi
ISO Data
Izod Impact, Notched (ISO) 4.00 kJ/m²
1.90 ft-lb/in²
ISO Test
Thermal Properties Metric English Comments
Melting Point 223 °C
433 °F
10 K/min
Deflection Temperature at 1.8 MPa (264 psi) 170 °C
338 °F
ISO 75
Descriptive Properties Value Comments
Color BK5830
Commercial Status Active America
Impact Modified No
Primary Processing Technique Injection Molding