Material Notes:
Car interior trim panels.Data was collected by ISO methods and provided by BASF.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
Linear Mold Shrinkage, Flow 0.011 cm/cm
0.011 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Yield 24.0 MPa
3480 psi
Tensile Modulus 2.20 GPa
319 ksi
Charpy Impact Unnotched 5.50 J/cm²
26.2 ft-lb/in²
2.00 J/cm²

@Temperature -30.0 °C
9.52 ft-lb/in²

@Temperature -22.0 °F
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 80.0 µm/m-°C

@Temperature 20.0 °C
44.4 µin/in-°F

@Temperature 68.0 °F
Deflection Temperature at 0.46 MPa (66 psi) 104 °C
219 °F
Deflection Temperature at 1.8 MPa (264 psi) 62.0 °C
144 °F
Vicat Softening Point 104 °C
219 °F