Material Notes:
Uses: Electrical appliance housings (e.g. drills), components requiring high impact and temperature resistance, furniture frames.Data was collected by ISO methods and provided by BASF.
Physical Properties Metric English Comments
Density 1.12 g/cc
0.0405 lb/in³
Linear Mold Shrinkage, Flow 0.0060 cm/cm
0.0060 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 61.0 MPa
8850 psi
Elongation at Break 3.5 %
3.5 %
Tensile Modulus 5.70 GPa
827 ksi
Charpy Impact Unnotched 6.00 J/cm²
28.6 ft-lb/in²
5.50 J/cm²

@Temperature -30.0 °C
26.2 ft-lb/in²

@Temperature -22.0 °F
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 30.0 µm/m-°C

@Temperature 20.0 °C
16.7 µin/in-°F

@Temperature 68.0 °F
Deflection Temperature at 0.46 MPa (66 psi) 159 °C
318 °F
Deflection Temperature at 1.8 MPa (264 psi) 140 °C
284 °F
Vicat Softening Point 95.0 °C
203 °F
Flammability, UL94 HB

@Thickness 0.750 mm
HB

@Thickness 0.0295 in