Material Notes:
Uses: car and truck fans and shrouds, car rear light housings, car radiator expansion tanks, car grills, domestic appliance components (e.g. washing machine tanks, impellers housings, etc.), textile bobbins and chemical plant, furniture frames.Data was collected by ISO methods and provided by BASF.
Physical Properties Metric English Comments
Density 1.12 g/cc
0.0405 lb/in³
Linear Mold Shrinkage, Flow 0.0060 cm/cm
0.0060 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 80.0 MPa
11600 psi
Elongation at Break 3.0 %
3.0 %
Tensile Modulus 7.50 GPa
1090 ksi
Charpy Impact Unnotched 3.50 J/cm²
16.7 ft-lb/in²
3.00 J/cm²

@Temperature -30.0 °C
14.3 ft-lb/in²

@Temperature -22.0 °F
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 30.0 µm/m-°C

@Temperature 20.0 °C
16.7 µin/in-°F

@Temperature 68.0 °F
Deflection Temperature at 0.46 MPa (66 psi) 160 °C
320 °F
Deflection Temperature at 1.8 MPa (264 psi) 148 °C
298 °F
Vicat Softening Point 144 °C
291 °F
Flammability, UL94 HB

@Thickness 0.750 mm
HB

@Thickness 0.0295 in