BASF Procom® GC20H 250 Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer BASF
Trade Name Procom®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Procom® GC20H 250 Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Uses: car and truck fans and shrouds, car rear light housings, car radiator expansion tanks, car grills, domestic appliance components (e.g. washing machine tanks, impellers housings, etc.), textile bobbins and chemical plant, furniture frames.Data was collected by ISO methods and provided by BASF.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
Linear Mold Shrinkage, Flow 0.0060 cm/cm
0.0060 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 70.0 MPa
10200 psi
Elongation at Break 3.0 %
3.0 %
Tensile Modulus 4.70 GPa
682 ksi
Charpy Impact Unnotched 3.50 J/cm²
16.7 ft-lb/in²
2.00 J/cm²

@Temperature -30.0 °C
9.52 ft-lb/in²

@Temperature -22.0 °F
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 40.0 µm/m-°C

@Temperature 20.0 °C
22.2 µin/in-°F

@Temperature 68.0 °F
Deflection Temperature at 0.46 MPa (66 psi) 160 °C
320 °F
Deflection Temperature at 1.8 MPa (264 psi) 142 °C
288 °F
Vicat Softening Point 130 °C
266 °F