Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

BASF Procom® D 1085 Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer BASF
Trade Name Procom®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Procom® D 1085 Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data was collected by ISO methods and provided by BASF.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
Linear Mold Shrinkage, Flow 0.0060 cm/cm
0.0060 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 65.0 MPa
9430 psi
Elongation at Break 3.5 %
3.5 %
Tensile Modulus 3.80 GPa
551 ksi
Charpy Impact Unnotched 4.00 J/cm²
19.0 ft-lb/in²
3.00 J/cm²

@Temperature -30.0 °C
14.3 ft-lb/in²

@Temperature -22.0 °F
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 40.0 µm/m-°C

@Temperature 20.0 °C
22.2 µin/in-°F

@Temperature 68.0 °F
Deflection Temperature at 0.46 MPa (66 psi) 145 °C
293 °F
Deflection Temperature at 1.8 MPa (264 psi) 130 °C
266 °F
Vicat Softening Point 107 °C
225 °F
Users viewing this material also viewed the following: