Material Notes:
Data was collected by ISO methods and provided by BASF.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
Linear Mold Shrinkage, Flow 0.015 cm/cm
0.015 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Yield 29.0 MPa
4210 psi
Elongation at Break 20 %
20 %
Tensile Modulus 2.00 GPa
290 ksi
Charpy Impact Unnotched 3.50 J/cm²
16.7 ft-lb/in²
1.00 J/cm²

@Temperature -30.0 °C
4.76 ft-lb/in²

@Temperature -22.0 °F
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 80.0 µm/m-°C

@Temperature 20.0 °C
44.4 µin/in-°F

@Temperature 68.0 °F
Deflection Temperature at 0.46 MPa (66 psi) 115 °C
239 °F
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °C
158 °F
Vicat Softening Point 100 °C
212 °F
Flammability, UL94 HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in