BASF Pluracol® Balance 50 Slabstock Foam Polyol

Category Fluid
Manufacturer BASF
Trade Name Pluracol®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Pluracol® Balance 50 Slabstock Foam Polyol.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Pluracol® Balance 50 polyol is a trifunctional polyether polyol based on a renewable raw material which contains mainly secondary hydroxyl groups. The polyol is capable of producing a broad range of flexible slabstock polyurethane foams, for furniture and bedding applications. This polyol has been formulated with a low emission antioxidant combination which is amine free.Information provided by BASF
Physical Properties Metric English Comments
Density 0.978 g/cc

@Temperature 54.5 °C
0.0353 lb/in³

@Temperature 130 °F
0.986 g/cc

@Temperature 43.4 °C
0.0356 lb/in³

@Temperature 110 °F
1.00 g/cc

@Temperature 25.0 °C
0.0361 lb/in³

@Temperature 77.0 °F
Viscosity 178 cP

@Temperature 54.5 °C
178 cP

@Temperature 130 °F
285 cP

@Temperature 43.4 °C
285 cP

@Temperature 110 °F
738 cP

@Temperature 25.0 °C
738 cP

@Temperature 77.0 °F
Molecular Weight 3000 g/mol
3000 g/mol
Chemical Properties Metric English Comments
Total Acid Number <= 0.060
<= 0.060
STI 3063/3161
Processing Properties Metric English Comments
Moisture Content <= 0.050 %
<= 0.050 %
STI 3062
Descriptive Properties Value Comments
Color Pale Yellow Liquid
Hydroxyl Number 47 - 53 mg KOH/g
STI 3007/3162