Material Notes:
Description: Pluracol® 945 polyol is a high molecular weight polyol for use in high water, low-density automotive seating foams where a high degree of foam stability is required. In combination with graft polyols, such as Pluracol 973, Pluracol 945 produces molded foams from high-water, low-density formulations. These foams are less susceptible to mold leakage, voiding and basal cells than foams produced with other polyols, but do require crushing to prevent shrinkage. Pluracol 945 is more reactive than either Pluracol 816 or Pluracol 538.Information provided by BASF
Physical Properties Metric English Comments
Density 1.00 g/cc

@Temperature 48.9 °C
0.0361 lb/in³

@Temperature 120 °F
1.01 g/cc

@Temperature 37.8 °C
0.0365 lb/in³

@Temperature 100 °F
1.02 g/cc

@Temperature 25.0 °C
0.0368 lb/in³

@Temperature 77.0 °F
Viscosity 270 cP

@Temperature 48.9 °C
270 cP

@Temperature 120 °F
370 cP

@Temperature 37.8 °C
370 cP

@Temperature 100 °F
850 cP

@Temperature 25.0 °C
850 cP

@Temperature 77.0 °F
Thermal Properties Metric English Comments
Specific Heat Capacity 1.16 J/g-°C
0.277 BTU/lb-°F
Thermal Conductivity 0.125 W/m-K
0.868 BTU-in/hr-ft²-°F
Chemical Properties Metric English Comments
Total Acid Number <= 0.010
<= 0.010
STI 3063/3161
Processing Properties Metric English Comments
Moisture Content <= 0.050 %
<= 0.050 %
STI 3062
Descriptive Properties Value Comments
Color <30
APHA, STI 3057
Clear Liquid
Composition Na & K
<5 ppm, STI 3038
Hydroxyl Number 34 - 36 mg KOH/g
STI 3007/3162
Unsaturation <0.05 meq/g
STI 3056