BASF Paliotol™ Yellow L 0962 Color Additive

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer BASF
Trade Name Paliotol™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Paliotol™ Yellow L 0962 Color Additive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Opaque quinophthalone yellow with excellent rheologySuitable for: Baking systems, Waterborn systems, Acrylic-isocyanate systems, Acid curing system and Airdrying systemsInformation provided by BASF
Physical Properties Metric English Comments
Density 2.02 g/cc
0.0730 lb/in³
Specific Surface Area 15 m²/g
15 m²/g
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 250 °C
482 °F
Electrical Properties Metric English Comments
Electrical Resistivity >= 5000 ohm-cm
>= 5000 ohm-cm
Chemical Properties Metric English Comments
Total Acid Number 3.5 - 6.5
3.5 - 6.5
Descriptive Properties Value Comments
Chemical Fastness (months) Butylacetate
5
Ethanol
5
HCL 2%
5
Methyl ethyl ketone
4
Mineral spirits
5
NaOH 2%
5
Solvenon™PM
4-5
Xylene
4
Color Yellow
Fastness to Overcoating 5