BASF Paliotan® Yellow L 1240 Color Additive

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer BASF
Trade Name Paliotan®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Paliotan® Yellow L 1240 Color Additive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Economical lead free pigment with good hiding, high chroma and color strengthSuitable for: Baking systems
Physical Properties Metric English Comments
Density 2.30 g/cc
0.0831 lb/in³
Specific Surface Area 13 m²/g
13 m²/g
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 150 °C
302 °F
Electrical Properties Metric English Comments
Electrical Resistivity >= 2500 ohm-cm
>= 2500 ohm-cm
Chemical Properties Metric English Comments
Total Acid Number 6.0 - 8.0
6.0 - 8.0
Descriptive Properties Value Comments
Chemical Fastness (months) Butylacetate
3
Ethanol
4
HCL 2%
5
Methyl ethyl ketone
3
Mineral spirits
4
NaOH 2%
5
Solvenon™PM
2-3
Xylene
3
Color Yellow
Fastness to Overcoating 3