Material Notes:
Formula: C6H11NOCAS: 2687-91-4Description: N-Ethylpyrrolidone-2 (NEP) Is a colorless to yellow liquid, with an amine like odor. It is miscible in water and soluble in other organic solvents.Synonyms: NEP, N-Ethylpyrrolidone, 1-Ethyl-2-pyrrolidinone, N-Ethyl-2-pyrrolidinon, N-EthylpyrrolidinoneApplications: Intermediate used in the production of Cosmetic industry, Paint and printing ink industry, Paint strippers, Pharmaceuticals and Solvent/cleaner for polymeric residualInformation provided by BASF
Physical Properties Metric English Comments
Density 0.998 g/cc
0.0361 lb/in³
Molecular Weight 113.2 g/mol
113.2 g/mol
Thermal Properties Metric English Comments
Melting Point <= -75.0 °C
<= -103 °F
Boiling Point 212 °C
414 °F
Flash Point 91.0 °C
196 °F
Processing Properties Metric English Comments
Moisture Content <= 0.10 %
<= 0.10 %
DIN 51 777
Descriptive Properties Value Comments
Assay >99.4%
Color <50
APHA, DIN EN 1557
Ignition Temperature 245°C