BASF Lupranate® R2500 Isocyanate

Category Fluid
Manufacturer BASF
Trade Name Lupranate®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Lupranate® R2500 Isocyanate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Lupranate® R2500 Isocyanate is a polymeric MDI with a functionality of approximately 2.7. Careful control of the MDI distribution in Lupranate R2500 Isocyanate helps provide uniform reactivity. This isocyanate can be used for the production of rigid insulation foams by molding, spraying, and frothing. It is also used for rigid and semi-flexible integral skin foams. CASE applications include floor coatings and microcellular elastomers.Information provided by BASF
Physical Properties Metric English Comments
Density 1.23 g/cc
0.0444 lb/in³
Viscosity 190 cP
190 cP
Vapor Pressure 2.67e-7 bar

@Temperature 25.0 °C
0.000200 torr

@Temperature 77.0 °F
Thermal Properties Metric English Comments
Boiling Point >= 190 °C

@Pressure 0.000667 MPa
>= 374 °F

@Pressure 0.0967 psi
Flash Point 200 °C
392 °F
Descriptive Properties Value Comments
Color Dark Brown
Composition Hydrolyzable Chlorine
0.00035
NCO content
0.315