BASF Lupranate® 275 Isocyanate

Category Fluid
Manufacturer BASF
Trade Name Lupranate®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Lupranate® 275 Isocyanate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Lupranate® 275 Isocyanate is a 15.9% Free-NCO prepolymer based on diphenylmethane diisocyanate (MDI) chemistry. The formulation of Lupranate 275 Isocyanate provides the low viscosity and physical properties required for high-quality, fixed-ratio spray applications. Lupranate 275 Isocyanate is a zero-VOC prepolymer.Information provided by BASF
Physical Properties Metric English Comments
Density 1.15 g/cc
0.0415 lb/in³
Viscosity 560 cP
560 cP
Vapor Pressure 1.33e-8 bar

@Temperature 25.0 °C
0.00000998 torr

@Temperature 77.0 °F
Thermal Properties Metric English Comments
Boiling Point >= 190 °C

@Pressure 0.000667 MPa
>= 374 °F

@Pressure 0.0967 psi
Flash Point 200 °C
392 °F
Descriptive Properties Value Comments
Color Clear
Composition NCO content
0.159