BASF Lupranate® 273 Isocyanate

Category Fluid
Manufacturer BASF
Trade Name Lupranate®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Lupranate® 273 Isocyanate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Lupranate® 273 Isocyanate is a solvent-free polymeric MDI with a functionality of approximately 2.3. Lupranate® 273 Isocyanate is a polymeric MDI which contains a relatively high level of pure MDI. The low functionality and low viscosity of this product are found to be advantageous in formulating potting compounds, microcellular elastomers, and packaging foams. The combination of relatively fast reactivity with slower gel time makes this product an excellent choice for semi-flexible and integral skin foams where it is important to achieve short cycle times while obtaining good flow characteristics. Lupranate® 273 Isocyanate is also used with success in carpet backing, adhesive, and sealant applications.Information provided by BASF
Physical Properties Metric English Comments
Density 1.22 g/cc
0.0441 lb/in³
Viscosity 45 - 75 cP
45 - 75 cP
Vapor Pressure 2.67e-7 bar

@Temperature 25.0 °C
0.000200 torr

@Temperature 77.0 °F
Thermal Properties Metric English Comments
Boiling Point >= 190 °C

@Pressure 0.000667 MPa
>= 374 °F

@Pressure 0.0967 psi
Flash Point >= 200 °C
>= 392 °F
Descriptive Properties Value Comments
Color Dark Brown
Composition Hydrolyzable Chlorine
0.0003
NCO content
31.5-32.5%
Users viewing this material also viewed the following: