Material Notes:
Chemical Structure: Cu-Phthalocyanine, alphaPhysical form: PowderApplication: Pigment for PaintsInformation provided by BASF
Physical Properties Metric English Comments
Density 1.50 g/cc
0.0542 lb/in³
Specific Surface Area 63 m²/g
63 m²/g
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 300 °C
572 °F
Electrical Properties Metric English Comments
Electrical Resistivity >= 3333 ohm-cm
>= 3333 ohm-cm
Chemical Properties Metric English Comments
Total Acid Number 4.5 - 7.0
4.5 - 7.0
Descriptive Properties Value Comments
Chemical Fastness (months) Butylacetate
3
Ethanol
3-4
HCL 2%
5
Methyl ethyl ketone
1
Mineral spirits
4
NaOH 2%
5
Solvenon™PM
2
Xylene
3-4
Color Blue