Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

BASF Gusspolyamid® Nylon 6 (Dry As Molded)

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Unreinforced
Manufacturer BASF
Trade Name Gusspolyamid®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Gusspolyamid® Nylon 6 (Dry As Molded).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Processed by anionic polymerization of caprolactam in the presence of a catalyst and activator. Uses include semi-finished products and containers (e.g. heating oil tanks).Data was collected by ISO methods and provided by BASF.
Physical Properties Metric English Comments
Density 1.15 g/cc
0.0415 lb/in³
Water Absorption 8.0 %
8.0 %
Moisture Absorption at Equilibrium 2.8 %
2.8 %
Mechanical Properties Metric English Comments
Tensile Strength, Yield 95.0 MPa
13800 psi
Elongation at Break 50 %
50 %
Elongation at Yield 4.0 %
4.0 %
Tensile Modulus 4.00 GPa
580 ksi
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 70.0 µm/m-°C

@Temperature 20.0 °C
38.9 µin/in-°F

@Temperature 68.0 °F
Melting Point 220 °C
428 °F
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
Dielectric Constant 3.7

@Frequency 1e+6 Hz
3.7

@Frequency 1e+6 Hz
Dissipation Factor 0.030

@Frequency 1e+6 Hz
0.030

@Frequency 1e+6 Hz
Comparative Tracking Index 600 V
600 V