Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

BASF Elastollan R 2001 20% Glass Filled TPUR

Category Polymer , Thermoplastic , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced , Thermoplastic Polyurethane (TPUR), Polyester Grade
Manufacturer BASF
Trade Name Elastollan
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Elastollan R 2001 20% Glass Filled TPUR.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expansion comparable with steel and aluminum, low mold shrinkage and ease of painting. Typical Applications: Automotive body and rocker panels, underbody sealants, technical moldings e.g. plugs and ski tips.Note: Quoted results are from measurements on injection molded test platens, post tempered for 20 hours at 100°CInformation provided by BASF
Physical Properties Metric English Comments
Density 1.37 g/cc
0.0495 lb/in³
ISO 1183-1-A
Mechanical Properties Metric English Comments
Hardness, Shore D 67
67
ISO 686
Tensile Strength 60.0 MPa
8700 psi
50 mm/min; ISO 37
Elongation at Break 30 %
30 %
50 mm/min; ISO 37
Modulus of Elasticity 1.80 GPa
261 ksi
DIN EN ISO 527
Charpy Impact Unnotched 11.0 J/cm²

@Temperature -30.0 °C
52.3 ft-lb/in²

@Temperature -22.0 °F
DIN ISO 179
18.0 J/cm²

@Temperature 23.0 °C
85.7 ft-lb/in²

@Temperature 73.4 °F
DIN ISO 179
Charpy Impact, Notched 1.00 J/cm²

@Temperature -30.0 °C
4.76 ft-lb/in²

@Temperature -22.0 °F
DIN ISO 179
5.00 J/cm²

@Temperature 23.0 °C
23.8 ft-lb/in²

@Temperature 73.4 °F
DIN ISO 179
Thermal Properties Metric English Comments
CTE, linear 22.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
12.2 µin/in-°F

@Temperature 73.4 - 176 °F
53752-A
Deflection Temperature at 0.46 MPa (66 psi) 150 °C
302 °F
DIN EN ISO 75-2/Be
Deflection Temperature at 1.8 MPa (264 psi) 120 °C
248 °F
DIN EN ISO 75-2/Ae
Processing Properties Metric English Comments
Processing Temperature 225 - 245 °C
437 - 473 °F
Mold Temperature 50.0 - 70.0 °C
122 - 158 °F
Descriptive Properties Value Comments
Color Black
Commercial Status North America
Primary Processing Technique Injection molding
Users viewing this material also viewed the following: