BASF Elastollan C 75 A TPUR

Category Polymer , Thermoplastic , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyester Grade
Manufacturer BASF
Trade Name Elastollan
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Elastollan C 75 A TPUR.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and chemical resistance, outstanding wear resistance, high tear and tensile strength, good damping characteristics and a high resilience performance.Typical Applications: Spiral tubing, pneumatic tubing, round and v-belting, technical moldings, e.g. bushes, dust caps, seals, blow molding bellows, and mining screens.Note: Quoted results are from measurements on injection molded test platens, post tempered for 20 hours at 100°CInformation provided by BASF
Physical Properties Metric English Comments
Density 1.18 g/cc
0.0426 lb/in³
ISO 1183-1-A
Mechanical Properties Metric English Comments
Hardness, Shore A 80
80
ISO 868
Tensile Strength 35.0 MPa
5080 psi
after storage in water at 80°C for 42 days; ISO 37
50.0 MPa
7250 psi
ISO 37
2.00 MPa

@Strain 20.0 %
290 psi

@Strain 20.0 %
ISO 37
4.00 MPa

@Strain 100 %
580 psi

@Strain 100 %
ISO 37
7.50 MPa

@Strain 300 %
1090 psi

@Strain 300 %
ISO 37
Elongation at Break 650 %
650 %
ISO 37
650 %
650 %
after storage in water at 80°C for 42 days; ISO 37
Charpy Impact, Notched NB

@Temperature -30.0 °C
NB

@Temperature -22.0 °F
DIN EN ISO 179
NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
DIN EN ISO 179
Tear Strength 60.0 kN/m
342 pli
DIN ISO 34-1/Bb
Abrasion 30
30
[mm<sup>3</sup>; ISO 4649
Compression Set 25 %

@Temperature 23.0 °C
25 %

@Temperature 73.4 °F
ISO 815
35 %

@Temperature 70.0 °C
35 %

@Temperature 158 °F
ISO 815
Processing Properties Metric English Comments
Processing Temperature 160 - 220 °C
320 - 428 °F
Extrusion
170 - 240 °C
338 - 464 °F
Injection molding
Mold Temperature 20.0 - 70.0 °C
68.0 - 158 °F
Descriptive Properties Value Comments
Commercial Status North America
Primary Processing Technique Injection molding and Extrusion