BASF Elastollan 590 A TPUR

Category Polymer , Thermoplastic , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyester Grade
Manufacturer BASF
Trade Name Elastollan
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Elastollan 590 A TPUR.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and a high abrasion resistance.Typical Applications: Heel top-pieces, castor tyres and parts requiring a high durability.Note: Quoted results are from measurements on injection molded test platens, post tempered for 20 hours at 100°CInformation provided by BASF
Physical Properties Metric English Comments
Density 1.25 g/cc
0.0452 lb/in³
ISO 1183-1-A
Mechanical Properties Metric English Comments
Hardness, Shore A 94
94
ISO 868
Hardness, Shore D 41
41
ISO 686
Tensile Strength 50.0 MPa
7250 psi
ISO 37
Elongation at Break 600 %
600 %
ISO 37
Tear Strength 100 kN/m
571 pli
DIN ISO 34-1/Bb
Abrasion 35
35
[mm<sup>3</sup>; ISO 4649
Processing Properties Metric English Comments
Processing Temperature 175 - 230 °C
347 - 446 °F
Mold Temperature 20.0 - 70.0 °C
68.0 - 158 °F
Descriptive Properties Value Comments
Commercial Status North America
Primary Processing Technique Injection molding