Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

BASF Capron® 8351 Impact Modified Nylon 6 (Conditioned)  (discontinued **)

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Impact Grade
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Capron® 8351 Impact Modified Nylon 6 (Conditioned)  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Capron 8351 is a type 6 polyamide graft copolymer developed for injection molding applications requiring a high level of toughness combined with moderate flexibility and faster cycles. It is also available in heat stabilized (Capron 8351 HS) and/or pigmented versions.Capron 8351 is generally recommended for applications such as storage bins, spray gun and power tool handles, trim clips and fasteners, wall anchors, and automotive roof racks.Data provided by Allied Signal.Processing: Max. water content 0.2%. Product is supplied in sealed containers and drying is not required. If drying becomes necessary, a dehumidifying or desiccant dryer operating at 85°C (185 °F). Is recommended. Drying time is dependent on moisture level.Melt Temperature: 240-270 degC (464-518 degF). Mold Temperature: 80-95 degC (176-203 degF). Injection and Packing Pressure: 35-125 bar (500-1500psi) A mold temperature of 80-95 degC (176-203 degF) is recommended, but temperatures of 10-95 degC (50-203 degF) can be used where applicable. Injection pressure controls the filling of the part and should be applied for 90% of ram travel. Packing pressure affects the final part and can be used effectively in controlling sink marks and shrinkage. It should be applied and maintained until the gate area is completely frozen off. Fast fill rates are recommended to insure uniform melt delivery to the cavity and prevent premature freezing. Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line.
Physical Properties Metric English Comments
Density 1.07 g/cc
0.0387 lb/in³
(Dry)
Linear Mold Shrinkage 0.014 cm/cm
0.014 in/in
ASTM Data MD (Dry)
Linear Mold Shrinkage, Transverse 0.019 cm/cm
0.019 in/in
ISO Data (Dry)
Mechanical Properties Metric English Comments
Tensile Strength, Yield 33.0 MPa
4790 psi
ISO value at 50 mm/min.
35.0 MPa
5080 psi
ASTM value at 50 mm/min.
Elongation at Break >= 50 %
>= 50 %
Nominal
>= 100 %
>= 100 %
Nominal
Elongation at Yield 10 %
10 %
ASTM Value at 50 mm/min.
12 %
12 %
ISO Value at 50 mm/min.
Flexural Yield Strength 30.0 MPa
4350 psi
ASTM Data
Flexural Modulus 0.620 GPa
89.9 ksi
ASTM Data
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
(Dry)
Processing Properties Metric English Comments
Processing Temperature 280 °C
536 °F
See Materials Notes
Mold Temperature 70.0 °C
158 °F
See Materials Notes
Drying Temperature 85.0 °C
185 °F
See Materials Notes