Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

BASF Capron® 8224 HSL Nylon 6 (Conditioned)  (discontinued **)

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Unreinforced
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Capron® 8224 HSL Nylon 6 (Conditioned)  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by BASF Corporation.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line.
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
(DAM); ISO 1183
Water Absorption 1.6 %
1.6 %
24 hr. (DAM); ISO 62
9.5 %
9.5 %
(Beginning DAM); ISO 62
Moisture Absorption at Equilibrium 2.7 %
2.7 %
23°C/50% R.H. (Beginning DAM); ISO 62
Mechanical Properties Metric English Comments
Tensile Strength, Yield 40.0 MPa
5800 psi
2 in/min; ASTM D638
100 MPa

@Temperature -40.0 °C
14500 psi

@Temperature -40.0 °F
ISO 527
Elongation at Break >= 50 %
>= 50 %
50 mm/min; Nominal; ISO 527
>= 100 %
>= 100 %
2 in/min; ASTM D638
Flexural Strength 38.0 MPa
5510 psi
ASTM D790
170 MPa

@Temperature -40.0 °C
24700 psi

@Temperature -40.0 °F
ASTM D790
Flexural Modulus 0.760 GPa
110 ksi
ASTM D790
Izod Impact, Notched 0.800 J/cm
1.50 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
10 K/min (DAM)
220 °C
428 °F
(DAM); ASTM D3418
Descriptive Properties Value Comments
Additive Unfilled
Attribute Heat stabilized or stable to heat
Color Natural
Commercial Status (March 2007) Active America
Form Pellets
Impact Modified No
Other Extrusion Processable
Primary Processing Technique Wire and Cable
Profile extrusion Processable
UL.UL-C Yes