Formula: C7H12O2CAS: 141-32-2Description: Acrylic acid ester, for manufacturing polymers and for use as a feedstock for syntheses.Applications: Butyl acrylate forms homopolymers and copolymers. Copolymers of butyl acrylate can be prepared with acrylic acid and its salts, amides and esters, and with methacrylates, acrylonitrile, maleic acid esters, vinyl acetate, vinyl chloride, vinylidene chloride, styrene, butadiene, unsaturated polyesters and drying oils, etc. Butyl acrylate is also a very useful feedstock for chemical syntheses, because it readily undergoes addition reactions with a wide variety of organic and inorganic compound.Information provided by BASF
Physical Properties Metric English Comments
Density 0.898 g/cc
0.0324 lb/in³
Viscosity Measurement 0.92
0.92
[mPa.s}
Molecular Weight 128.2 g/mol
128.2 g/mol
Vapor Pressure 0.00540 bar
4.05 torr
Thermal Properties Metric English Comments
Specific Heat Capacity 1.93 J/g-°C
0.461 BTU/lb-°F
of liquid
Melting Point -64.0 °C
-83.2 °F
Freezing Point
Boiling Point 148 °C
298 °F
Optical Properties Metric English Comments
Refractive Index 1.4185
1.4185
Processing Properties Metric English Comments
Moisture Content <= 0.050 %
<= 0.050 %
ASTM E203
Descriptive Properties Value Comments
Acidity, as HCI 0.01
as acrylic acid, ASTM D1613
Assay >99.5%
Color <10
APHA, ASTM D1209
Heat of Polymerization 504 kJ/kg
Latent Heat of Evaporation at Boiling Point 292 kJ/kg
Standard Stabilization 10 - 20 ppm
MEHQ, ASTM D3125