Formula: C5H8N2CAS: 5877-42-9Description: Ethyloctinol is a colorless to yellowish liquid, with a perceptible odor.Synonyms: EthyloctinolApplications: Ideal for applications in Oilfield corrosion inhibitor and An intermediate precursorInformation provided by BASF
Physical Properties Metric English Comments
Density 0.870 g/cc
0.0314 lb/in³
Molecular Weight 154.3 g/mol
154.3 g/mol
Thermal Properties Metric English Comments
Melting Point -45.0 °C
-49.0 °F
Boiling Point 205 °C
401 °F
Flash Point 84.0 °C
183 °F
Descriptive Properties Value Comments
Assay >98%
Ignition Temperature 265°C