Material Notes:
Reinforced with 40% bronze for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Physical Properties Metric English Comments
Density 3.20 g/cc
0.116 lb/in³
ISO 1183
Filler Content 40 %
40 %
Bronze Filler
Particle Size 40 µm
40 µm
Average
Mechanical Properties Metric English Comments
Hardness, Shore D 61
61
ISO 868
Ball Indentation Hardness 40.0 MPa
5800 psi
ISO 2039-1
Tensile Strength, Yield 17.0 MPa
2470 psi
ISO 527
Elongation at Break 260 %
260 %
ISO 527
Izod Impact, Notched 1.40 J/cm
2.62 ft-lb/in
ISO 180
Thermal Properties Metric English Comments
CTE, linear 65.0 µm/m-°C

@Temperature 20.0 °C
36.1 µin/in-°F

@Temperature 68.0 °F
ASTM E 831
Melting Point 327 °C
621 °F
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Volume Resistivity 8.10e+16 ohm-cm
8.10e+16 ohm-cm
IEC 60093
Surface Resistance 5.50e+16 ohm
5.50e+16 ohm
IEC 60093
Dielectric Strength 10.0 kV/mm
254 kV/in
IEC 60243-1
Dissipation Factor 0.0020
0.0020
IEC 60250
Processing Properties Metric English Comments
Processing Temperature 360 °C
680 °F
Molding
Back Pressure 50.0 - 70.0 MPa
7250 - 10200 psi
Molding Pressure